Anybody know if ammonium fluoride in a neutral pH environment (i.e. without adding HF or additional acid to effectively form HF in solution from H+ and F- ions) will attack silicon dioxide or nitride at any appreciable rate?

Or more generally, tips on tuning a wet oxide etch to be as non-corrosive as possible to metals (specifically Al and Cu)?